YarnTwisting Twisting, winding and coating consulting

Why yarn breaks during twisting, and how to find the cause

End breaks are a symptom. The pattern of where and when they happen points straight at the cause, if you record it.

Start by recording, not adjusting

The instinct is to drop the speed or back off the tension and see if it helps. That hides the cause and costs output. Spend one shift recording every break instead:

  • Which spindle
  • Where in the yarn path the break happened
  • How full the feed package and the take-up package were
  • What the broken end looks like

Four patterns come out of that record, and each one narrows the search.

Pattern Most likely cause
The same few spindles, again and again Mechanical fault on those positions
All spindles, spread evenly Settings, material or climate
Mostly at one stage of the package Tension changing as the package builds or empties
Comes and goes with the lot or the weather Feed yarn quality or humidity

Reading the broken end

  • A clean, sharp end means the yarn was cut or snapped by a sudden tension peak. Look for a damaged guide, a snag on the feed package or a catch in the balloon.
  • A long tapered end on a staple yarn means the fibres slipped apart. There was a weak, low twist place in the feed yarn, or tension was high for a yarn that has not yet received its twist.
  • A fused or glazed end on a synthetic yarn means heat from friction. Look for a worn guide, a traveller running too hot or yarn rubbing on a balloon limiter.
  • A frayed end with broken filaments further back means abrasion over a length of the path, not a single point.

Tension and the balloon

On any spindle twister, the yarn swings around the spindle as a balloon. Balloon tension rises steeply with spindle speed, roughly with the square of it, so a ten percent speed increase adds about twenty percent to tension. It also rises with yarn weight and balloon size.

If breaks arrived with a speed increase, tension is the likely reason. The fix is rarely to give the speed back. Check first whether the balloon can be controlled with the limiter or guide height, and whether the tensioner setting still suits the new speed.

On a two-for-one twister, tension is set inside the spindle by the capsule or ball tensioner, and the yarn wraps part way around the storage disc before it rises into the balloon. Too little tension and the wrap grows until the yarn laps and breaks. Too much and the wrap disappears, the balloon collapses and tension peaks reach the yarn directly. The wrap angle on the storage disc is the thing to watch, and it should stay steady from a full feed package to an empty one.

On a ring twister, the traveller is the tensioner. Its weight has to suit the yarn count and the spindle speed. Too light and the balloon is large and unstable. Too heavy and tension is high all the time. Worn travellers and worn rings give an erratic drag that shows as breaks on particular positions.

Machine condition

Breaks that stay with a spindle are mechanical until proved otherwise. Work along the yarn path:

  1. Guides and eyelets. Run a fingernail or a length of fine yarn around every ceramic. A groove you can feel will cut yarn.
  2. Tensioners. Check for fluff, finish build up and worn surfaces.
  3. Spindle. Look for vibration, a bent blade or a slack drive tape. A slow spindle also gives low twist.
  4. Balloon limiter and separators. Look for rub marks and burrs.
  5. Take-up. Check traverse guides, the drum surface and cradle pressure.

Swapping the feed package to a good spindle is a quick test. If the breaks follow the package, it is the yarn. If they stay with the spindle, it is the machine.

Feed packages

A twister can only run as well as its supply unwinds. Common faults:

  • Ribboning on the feed package, which makes the yarn pluck off in jerks. See the guide to ribboning.
  • Sloughing, where several wraps come off together.
  • Poor knots or splices that will not pass the tensioner.
  • Uneven density from assembly winding, which gives one end tight and one slack. In the twisted yarn this shows as a corkscrew, and the tight end carries the load and breaks.

On two-for-one machines the quality of the assembly wound feed package matters more than almost anything else.

Twist level

For staple yarns, too little twist leaves the yarn weak at the point where tension is highest. Too much twist makes it lively, so it snarls at every slack moment and the snarl breaks when it reaches a guide. Check that the twist is right for the count with the twist multiplier calculator, and check the real twist with a twist tester instead of trusting the setting.

Climate

Dry air raises static on synthetics and makes cotton and other natural fibres weaker and more brittle. If breaks follow the weather, or get worse when heating or air conditioning comes on, measure humidity in the room before changing the machine.

When to get help

If a shift of recording does not show a pattern, or the pattern points to something you cannot see, a second pair of eyes usually finds it quickly. Paul offers twisting consulting for exactly this, often starting from photos and your break record.

Tell Paul what the machine is doing

Send the yarn, the machine and the problem. You will get a straight answer on whether it can be fixed on the equipment you have, and what it would take.

Send an enquiry